3.jpg
2.jpg
1.jpg
3.jpg
2.jpg
1.jpg

301-1.4310-X10CrNi18.8

Specification:

ASTM F899

Introduce:

Stainless steel with austenitic organisation at room temperature becomes austenitic stainless steel, the chromium content is generally between 16% and 26%. Austenite mainly rely on cold working to strengthen the hardness, because of its low carbon content, welding performance is better, corrosion resistance is also very good. It has excellent corrosion resistance, and is used in conventional medical devices, such as: puncture products, handles, and non-critical parts of the product.

Chemical Composition(%)

Carbon,maxAManganesePhosphorus MaxSulfurSilicon MaxAChromiumNickelOther Elements
0.152.00 max0.0450.030 max1.0016.00-18.006.00-8.00-

Available in  bars 

Stock Specificationsφ3.0-100mmDelivery conditionsolid state
UT Detection Standards IncludeAA, A1, A, and BSurfacepolished bars, double-end chamfering
Toleranceh6-h9 level (customizable)Length3M/piece (customizable length)

Available in  plates 

Stock Specificationsδ0.8-200mmDelivery conditionsolid state
UT Detection Standards IncludeAA, A1, A, and BSurfacebright surface, free from burrs
Tolerance0/+0.3mm (customizable)Length250*500MM/PCS (width/length customizable)

Sample Display

If you need any of the above mentioned products, we can supply them directly and process the products according to your needs.